Water-based Formulated Blend Polyols for Polyurethane PIR Block Foam
Reaction properties (hand test)
Item | Unit | Specification |
DmcBlock 1861 PIR | g | 100 |
DmcIso 1800 | g | 140-160 |
Cream time | sec | 40-50 |
Gel time | sec | 200-220 |
Free rise density | kg/m3 | 42-44 |
Item | Unit | Specification | Test standard |
Core density | kg/m3 | ≥40 | ASTM D1622-08 |
Thermal conductivity, 10ºC | W/(m.k) | ≤0.030 | ASTM C518-10 |
Compressive strength | Kpa | ≥200 | ASTM D1621-10 |
Tensile strength | Kpa | ≥270 | |
Closed cell content | % | ≥90 | ASTM D6226 |
Thermal stability, -30-80ºC | % | ≤1.0 | ASTM D2126-09 |
Flammability | / | B2 | DIN 4102 |
The above testing data have been generated in lab or field conditions which are typical for this application. They are believed to be correct but data variations due to varying processing or ambient conditions can not be excluded. The customer remains responsible for making his own interpretation of data and suitability of the chemicals to his particular operation.
220kg/drum for Polyol and 250kg/drum for Isocyanate.